Project Description

Commitment to You

We are committed to integrate steel resources in china and serve the global steel market. We have 15+ years of experience in steel researching, production, managing and sales.

Our ability to purchase materials directly from leading mills will give you the competitive edge. Any Questions Just Call +86-731-89903933

430 1.4016 is a non-hardenable steel containing straight chromium, and belongs to the ferritic group of steels. This steel is known for its good corrosion resistance and formability, coupled with practical mechanical properties. It can be used in certain chemical applications due to its resistance to nitric acid.

430F 1.4510 is a ferritic, straight chromium alloy melted as AOD. This alloy is similar to 430 stainless with increased sulfur to dramatically improve machinability This alloy does not form as easily as standard 430 due to the sulfur but still has moderate ductility.

430Ti 1.4510 is a medium-chromium ferritic stainless steel that can be used in many mildly corrosive environments.

Applications  

  • Dish washer linings
  • Refrigerator cabinet panels
  • Element supports and fasteners
  • Stove trim rings and chimney liners
  • Automotive trim and lashing wires

Comparison

STANDARD UNS JIS WERKSTOFF NR. EN
430 S43000 SUS430 1.4016 X6Cr17
430F S43020 SUS430F 1.4104 X14CrMoS17
430Ti S43036 SUS 430LX 1.4510 X3CrTi17

Chemical Composition

Grade C Mn Si P S Cr Ni
430 min.

max.

0.12

1

1

0.04

0.030

16

18

0.50

430F min.

max.

0.12

1.25

1

0.06

0.15

16

18

430Ti min.

max.

0.05

1

1

0.04

0.015

16

18

Ti 0.15-0.8

Mechanical Properties

Grade Tensile Strength (MPa) min Yield Strength 0.2% Proof (MPa) min Elongation (% in 50mm) min Hardness
Rockwell B (HR B) max Brinell (HB) max
430 483 310 22 85 183
430F 552 typical 379 typical 25 typical 262
430Ti 515 310 30 255

Sizes

Hot Rolled Process – OD 30-500mm ; WT 3-60mm ; L 6-12meter

Cold Drawn Process – OD 10-200mm ; WT 0.5-20mm ; L 1-12meter

Cold Rolled Process – OD 6-200mm ; WT 0.1-20mm ; L 1-12meter

Surface

Acid pickling – pre-passivation process of treating stainless steel parts with an acid solution, typically hydrochloric or sulfuric acid, which can remove oxide scale and heat tint while dissolving steel flecks embedded in the part.

Polishing – P grade sandpaper: P150, P200, P250, P300, P400, P500, P600, P700, P800

Inspection

Chamical analysis / Tensile test at room temperature / flattening test / ring tensile test / drift expemdomg test / ring expanding test / leak tightness test / Tensile test at elevated temperature / impact test at room temperature / impact test at low temperature / eddy current test / ultrasonic test / magnetic flux leakage test

Corrosion Resistance

All ferritic grades, such as stainless steel grade 430, have excellent stress corrosion cracking resistance. Grade 430 has good corrosion resistance to numerous substances, such as certain organic acids and nitric acid. The corrosion resistance is maximized in well-polished or buffed condition. Its pitting and crevice corrosion resistance is quite similar to that of grade 304. 430F is a high-sulfur free machining grade, and therefore the resistance to pitting and crevice corrosion is comparatively lesser than those grades that are non-free machining.

Heat Resistance

Stainless steel grade 430 is capable of resisting oxidation up to 870°C (1598°F) in intermittent usage, and up to 815°C (1499°F) in continuous usage. At room temperature, it has the tendency to become brittle, especially when it has been heated for a long time in the 400-600°C (752-1112°F) range. This issue can be overcome with annealing.

Heat Treatment

Solution annealing can be performed by heating stainless steel grade 430 to 815 – 845°C (1499-1553°F). Then it has to be slow furnace cooled to 600°C (1112°F) and followed by air-cooling in a quick manner – as slow cooling between 540 and 400°C (1004 and 752°F) tends to cause embrittlement.

For sub-critical annealing, heating should be performed to 760-815°C (1400-1499°F), followed by air-cooling or water quenching.

Welding

To perform any welding, stainless steel grade 430 has to be pre-heated at 150-200°C (302-392°F). In case of embrittlement in the welded metal, the particular area can be post-weld annealed at 790-815°C (1454-1499°F); however grain refinement will not happen.

Machining

The machinability of stainless steel grade 430 is a lot easier than standard austenitic steels such as grade 304 – but there is a chance for galling. Lightly drawn bars are easier to machine than bars in the annealed condition. Grade 430F is easy to machine.

Fabrication

Stainless steel grade 430 has a low work hardening rate which enables easy bending and forming. The low ductility rate, however, makes it difficult to perform very rigorous operations. It is possible for grade 430 wire to handle rigorous cold heading. Sub-critical intermediate annealing may be required for extreme cold working.

Experienced 15+ Years

Our ability to purchase materials directly from leading mills at the best possible price will give you the competitive edge. This coupled with a skilled workforce dedicated to embracing the demands of the markets.

We Can Supply Follows Products with High Quality:

  1. Cold Rolled Steel Tube
  2. Cold Drawn Steel Tube
  3. Hollow Bar
  4. Honed Tube
  5. Plated Tube
  6. Plated Bar
  7. Boiler Tube

All Products According Quality Standard Strictly:

  1. ASTM: ASTM A519, ASTM A513.
  2. JIS:JIS G3441, JIS G3445, JIS G3466, JIS G3459.
  3. DIN: DIN1626, DIN1629, DIN2391, DIN2393, DIN2448, DIN2458.
  4. EN: EN10305.
  5. BS: BS6323.

Wide Range of Pipes to Fit Your Industry:

  1. OD from 5mm to 820mm.
  2. Wall Thickness from 0.1 to 100mm.
  3. Length up to 50mtr per pc.

    Your Name *

    Your Email *

    Company Name

    Phone Number *

    Further Information

    Can’t Find What You Looking for? Check Popular Items Blew.

    Direct from the Source and Deliver to You in a Very Fast and Efficient Timeframe.